EN 573-3 AW-5005A H112 – Voedselveilige Aluminium-Magnesiumlegering
Natureel gehard AlMg-legering. Deze legering is voedselveilig.
Eigenschappen
Algemeen
| Eigenschap | Temperatuur | Waarde | Toestand | Gerelateerde Normen | Vorm |
|---|---|---|---|---|---|
| Dichtheid | 2,69 g/cm³ | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | |
| 20,0 °C | 2,69 g/cm³ | H112 | EN 573-3 | Profiel, Staaf, Buis | |
| 20,0 °C | 2,69 - 2,7 g/cm³ | H112 | EN 573-3 | Profiel, Staaf, Buis | |
| 20,0 °C | 2,7 g/cm³ | H112 | EN 573-3 | Profiel, Staaf, Buis |
Mechanisch
| Eigenschap | Temperatuur | Waarde | Toestand | Gerelateerde Normen | Vorm | Opmerking |
|---|---|---|---|---|---|---|
| Elasticiteitsmodulus | 69,5 GPa | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | ||
| 20,0 °C | 69,5 GPa | H112 | EN 573-3 | Profiel, Staaf, Buis | ||
| Rek | 16,0 % | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | A50 | |
| 18,0 % | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | A100 | ||
| 20,0 °C | 16,0 % | H112 | EN 573-3 | Profiel, Buis, Staaf | A50 | |
| 20,0 °C | 18,0 % | H112 | EN 573-3 | Profiel, Buis, Staaf | ||
| Hardheid, Brinell | 20,0 °C | 30,0 [-] | H112 | EN 573-3 | Profiel, Buis, Staaf | |
| Vlaaksbreukzwaarte | 22,0 - 35,0 MPa·√m | Typisch voor gewalste 5000-serie aluminium | ||||
| Poissonverhouding | 20,0 °C | 0,33 [-] | H112 | EN 573-3 | Profiel, Staaf, Buis | |
| Schuifmodulus | 26,1 GPa | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | ||
| 20,0 °C | 25,0 - 26,1 GPa | H112 | EN 573-3 | Profiel, Staaf, Buis | ||
| 20,0 °C | 26,1 GPa | H112 | EN 573-3 | Profiel, Staaf, Buis | ||
| Treksterkte | 100,0 MPa | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | ||
| 20,0 °C | 100,0 MPa | H112 | EN 573-3 | Profiel, Buis, Staaf |
Thermisch
| Eigenschap | Temperatuur | Waarde | Toestand | Gerelateerde Normen | Vorm | Opmerking |
|---|---|---|---|---|---|---|
| Uitzettingscoëfficiënt | -50 °C | 2,18e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | |
| -50,0 °C | 2,18e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 20 °C | 2,18e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 20 °C | 2,36e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 20 °C | 2,45e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 20 °C | 2,55e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 100 °C | 2,36e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 100,0 °C | 2,36e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 200 °C | 2,45e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 200,0 °C | 2,45e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 300 °C | 2,55e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| 300,0 °C | 2,55e-05 1/K | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | ||
| Max. diensttemperatuur | 150,0 °C | Typisch voor gewalste 5000-serie aluminium | ||||
| Smeltpunt | 630,0 - 650,0 °C | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | ||
| Specifieke warmtecapaciteit | 20,0 °C | 879,0 J/(kg·K) | H112 | EN 573-3 | Profiel, Staaf, Buis | |
| 20,0 °C | 879,0 - 899,0 J/(kg·K) | H112 | EN 573-3 | Profiel, Staaf, Buis | ||
| 20,0 °C | 899,0 J/(kg·K) | H112 | EN 573-3 | Profiel, Staaf, Buis | ||
| Warmtegeleiding | 20,0 °C | 160,0 - 220,0 W/(m·K) | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf, Profiel, Staaf | |
| 20,0 °C | 160,0 - 201,0 W/(m·K) | H112 | EN 573-3 | Profiel, Staaf, Buis | ||
| 20,0 °C | 201,0 - 220,0 W/(m·K) | H112 | EN 573-3 | Profiel, Staaf, Buis | ||
| 20,0 °C | 201,0 W/(m·K) | H112 | EN 573-3 | Profiel, Staaf, Buis |
Elektrisch
| Eigenschap | Temperatuur | Waarde | Toestand | Gerelateerde Normen | Vorm |
|---|---|---|---|---|---|
| Elektrische geleidbaarheid | 20,0 °C | 23.000.000 - 31.000.000 S/m | H112 | EN 573-3, EN 755 | Profiel, Staaf, Buis, Strip, Blad, Plaat, Staaf |
| Elektrische weerstand | 3,23e-08 - 4,35e-08 Ω·m | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | |
| 20,0 °C | 3,3e-08 Ω·m | H112 | EN 573-3 | Profiel, Staaf, Buis |
Chemische samenstelling
| Element | Waarde | Toestand | Gerelateerde Normen | Vorm |
|---|---|---|---|---|
| Chroom | 0,1 % | H112 | EN 573-3, EN 755 | Profiel, Staaf, Buis, Strip, Blad, Plaat, Staaf |
| Koper | 0,05 % | H112 | EN 573-3, EN 755 | Profiel, Staaf, Buis, Strip, Blad, Plaat, Staaf |
| IJzer | 0,45 % | H112 | EN 573-3 | Profiel, Staaf, Buis |
| 0,45 % | H112 | EN 573-3, EN 755 | Strip, Blad, Plaat, Buis, Staaf | |
| Magnesium | 0,7 - 1,1 % | H112 | EN 573-3, EN 755 | Profiel, Staaf, Buis, Strip, Blad, Plaat, Staaf |
| Mangaan | 0,15 % | H112 | EN 573-3, EN 755 | Profiel, Staaf, Buis, Strip, Blad, Plaat, Staaf |
| Silicium | 0,3 % | H112 | EN 573-3, EN 755 | Profiel, Staaf, Buis, Strip, Blad, Plaat, Staaf |
| Zink | 0,2 % | H112 | EN 573-3, EN 755 | Profiel, Staaf, Buis, Strip, Blad, Plaat, Staaf |
Technologische eigenschappen
| Eigenschap | Beoordeling |
|---|---|
| Anodiseren | Decoratief: goed (EQ: zeer goed); Beschermend: zeer goed |
| Harden | Hard solderen (met/zonder vloeistof): voldoende - onvoldoende / voldoende; Wrijfsolderen: goed; Zacht solderen met vloeistof: acceptabel |
| Corrosie-eigenschappen | Zeeuwter: goed; Weerbestendigheid: zeer goed |
| Bewerkbaarheid | Buigen / Spinnen (koud): goed / acceptabel; Impactextrusie (koud): acceptabel; Dieptrekken / Opdikken (toestand) goed (O) / goed (H12) |
Metaal
- EN 573-3 Graad 3.3315 H112 – Uitgebreide Materialspecificaties
- EN 573-3 Graad 3.3326 H112 Aluminium – Dichtheid, Modulus, Sterkte & Normen
- EN 573-3 Gehalte 3.0285 H112: Uitgebreide materiaaleigenschappen
- EN 573-3 Gehalte 3.0515 H112 Aluminium – Belangrijkste eigenschappen en normen
- EN 573-3 Kwaliteit 3.3316 H112: Gedetailleerde Materiaaleigenschappen & Normen
- EN 573-3 Gehalte 3.0257 H112: Uitgebreide Aluminiumlegering Eigenschappen
- EN 573-3 Grade 3.0275 H112 – Premium Aluminiumlegering voor Gevorderde Toepassingen
- EN 573-3 Grade 3.3555 H112 – Specificaties en Kenmerken van Aluminiumlegering 5083
- EN 573-3 Grade 3.3525 H112 Aluminium: Eigenschappen en normen
- EN 573-3 Graad 3.0205 H112 – Gedetailleerde Eigenschappen & Standaarden
- EN 573-3 Graad 3.0255 H112 – Premium Aluminiumlegering voor Industriële Toepassingen